Standard Test Method for Oxidation Induction Time of Lubricating Greases by Pressure Differential Scanning Calorimetry

Standard Details

1.1 This test method covers the determination of oxidation induction time of lubricating greases subjected to oxygen at 3.5 MPa (500 psig) and temperatures between 155 °C and 210 °C.

1.2 Warning—The original data published in Research Report RR:D02-1314, was not analyzed in accordance the current D2PP. It also used instruments which are no longer manufactured and in a check of currently used instruments, none of the original instruments were still in use. The new precision of this test method is still to be established.

1.3 The values stated in SI units are to be regarded as standard. The values given in parentheses are for information only.

1.4 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety, health, and environmental practices and determine the applicability of regulatory limitations prior to use.

1.5 This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for the Development of International StandardDetails, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee.

General Information

Status : Historical
Standard Type: Main
Document No: ASTM D5483 : 20
Document Year: 2020
Pages: 5
  • Section Volume:
  • 05.02 Volume 05.02 Petroleum Products, Liquid Fuels, and Lubricants (II): D3711-D6122
  • ICS:
  • 75.100 Lubricants, industrial oils and related products

Life Cycle

Currently Viewing

Historical
ASTM D5483 : 20

Historical

Historical

Historical
Knowledge Corner

Expand Your Knowledge and Unlock Your Learning Potential - Your One-Stop Source for Information!

© Copyright 2026 BSB Edge Private Limited.

Enquire now +