1.1 This test method covers the determination of oxidation induction time of lubricating greases subjected to oxygen at 3.5 MPa (500 psig) and temperatures between 155 and 210°C.

1.2 The values stated in SI units are to be regarded as the standard.

1.3 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.

General Information

Status : Historical
Standard Type: Main
Document No: ASTM D5483 : 95
Document Year: 1995
Pages: 5
  • Section Volume:
  • 05.02 Volume 05.02 Petroleum Products, Liquid Fuels, and Lubricants (II): D3711-D6122
  • ICS:
  • 75.100 Lubricants, industrial oils and related products

Life Cycle

Historical

Currently Viewing

Historical
ASTM D5483 : 95
Knowledge Corner

Expand Your Knowledge and Unlock Your Learning Potential - Your One-Stop Source for Information!

© Copyright 2026 BSB Edge Private Limited.

Enquire now +