Standard Test Method for Measurement of Enthalpy of Fusion, Percent Crystallinity, and Melting Point of Ultra-High-Molecular Weight Polyethylene by Means of Differential Scanning Calorimetry

Standard Details

1.1 This test method discusses the measurement of the heat of fusion and the melting point of ultra-high-molecular weight polyethylene (UHMWPE), and the subsequent calculation of the percentage of crystallinity.

1.2 This test method can be used for UHMWPE in powder form, consolidated form, finished product, or a used product. It can also be used for irradiated or chemically-crosslinked UHMWPE.

1.3 This test method does not suggest a desired range of crystallinity or melting points for specific applications.

1.4 The values stated in SI units are to be regarded as the standard. The values given in parentheses are for information only.

1.5 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.

General Information

Status : Historical
Standard Type: Main
Document No: ASTM F2625 : 10
Document Year: 2010
Pages: 4
  • Section Volume:
  • 13.02 Volume 13.02 Medical and Surgical Materials and Devices (II): F2502-Latest; Emergency Medical Services; Search and Rescue; Anesthetic and Respiratory Equipment

Life Cycle

Currently Viewing

Historical
ASTM F2625 : 10
Knowledge Corner

Expand Your Knowledge and Unlock Your Learning Potential - Your One-Stop Source for Information!

© Copyright 2026 BSB Edge Private Limited.

Enquire now +