Standard Test Method for Measurement of Enthalpy of Fusion, Percent Crystallinity, and Melting Point of Ultra-High Molecular Weight Polyethylene by Means of Differential Scanning Calorimetry

Standard Details

1.1 This quantitative test method discusses the measurement of the heat of fusion and the melting point of ultra-high molecular weight polyethylene (UHMWPE), and the su

General Information

Status : ACTIVE
Standard Type: Main
Document No: ASTM F2625 : 24
Document Year: 2024
Pages: 5
  • Section Volume:
  • 13.02 Volume 13.02 Medical and Surgical Materials and Devices (II): F2502-Latest; Emergency Medical Services; Search and Rescue; Anesthetic and Respiratory Equipment

Life Cycle

Currently Viewing

ACTIVE
ASTM F2625 : 24

Historical

Historical
Knowledge Corner

Expand Your Knowledge and Unlock Your Learning Potential - Your One-Stop Source for Information!

© Copyright 2026 BSB Edge Private Limited.

Enquire now +