Plastics — Differential scanning calorimetry (DSC) — Part 2: Determination of glass transition temperature and glass transition step height

Standard Details

ISO 11357-2:2013 specifies methods for the determination of the glass transition temperature and the step height related to the glass transition of amorphous and partially crystalline plastics.

General Information

Status : WITHDRAWN
Standard Type: Main
Document No: ISO 11357-2:2013
Document Year: 2013
Pages: 6