Plastics — Differential scanning calorimetry (DSC) — Part 2: Determination of glass transition temperature and step height

Standard Details

This document specifies methods for the determination of the glass transition temperature and the step height related to the glass transition of amorphous and partially crystalline plastics.

General Information

Status : Published
Standard Type: Main
Document No: ISO 11357-2:2020
Document Year: 2020
Pages: 9
Edition: 3