This document specifies the methods for

a) uninterrupted creep tests with continuous monitoring of extension,

b) interrupted creep tests with periodic measurement of elongation,

c) stress rupture tests where normally only the time to fracture is measured,

d) a test to verify that a predetermined time can be exceeded under a given force, with the elongation or extension not necessarily being reported.

NOTE A creep test can be continued until fracture has occurred or it can be stopped before fracture.

General Information

Status : WITHDRAWN
Standard Type: Main
Document No: ISO 204:2018
Document Year: 2018
Pages: 53
Edition: 3

Life Cycle

Published

Currently Viewing

WITHDRAWN
ISO 204:2018

WITHDRAWN

WITHDRAWN
Knowledge Corner

Expand Your Knowledge and Unlock Your Learning Potential - Your One-Stop Source for Information!

© Copyright 2026 BSB Edge Private Limited.

Enquire now +