logo

Standards Manage Your Business

We Manage Your Standards

ISO

ISO 204:2023

Metallic materials — Uniaxial creep testing in tension — Method of test

Standard Details

This document specifies the methods for:

a)    uninterrupted creep tests with continuous monitoring of extension;

b)    interrupted creep tests with periodic measurement of elongation;

c)    stress rupture tests where normally only the time to fracture is measured;

d)    a test to verify that a predetermined time can be exceeded under a given force, with the elongation or extension not necessarily being reported.

NOTE       A creep test can be continued until fracture has occurred or it can be stopped before fracture.

General Information

Status : Published
Standard Type: Main
Document No: ISO 204:2023
Document Year: 2023
Pages: 48
Edition: 4

Life Cycle

Currently Viewing

Published
ISO 204:2023

WITHDRAWN

WITHDRAWN

WITHDRAWN
Knowledge Corner

Expand Your Knowledge and Unlock Your Learning Potential - Your One-Stop Source for Information!

© Copyright 2026 BSB Edge Private Limited.

Enquire now +