logo

Standards Manage Your Business

We Manage Your Standards

DIN

DVS 2203-4 : 1997

Testing of welded joints of thermoplastics plates and tubes - Tensible creep test

General Information

Status : WITHDRAWN
Standard Type: Main
Document No: DVS 2203-4 : 1997
Document Year: 1997