logo

Standards Manage Your Business

We Manage Your Standards

ASTM

ASTM E2009 : 23 New ASTM DRM Policy

Standard Test Methods for Oxidation Onset Temperature of Hydrocarbons by Differential Scanning Calorimetry

Standard Details

1.1 These test methods describe the determination of the oxidative properties of hydrocarbons by differential scanning calorimetry or pressure differential scanning calorimetry under linear heating rate conditions and are applicable to hydrocarbons, which oxidize exothermically in their analyzed form.

1.2 Test Method A—A differential scanning calorimeter (DSC) is used at ambient pressure of one atmosphere of oxygen.

1.3 Test Method B—A pressure DSC (PDSC) is used at high pressure (e.g., 3.5 MPa (500 psig) of oxygen).

1.4 Test Method C—A differential scanning calorimeter (DSC) is used at ambient pressure of one atmosphere of air.

1.5 Units—The values stated in SI units are to be regarded as standard. No other units of measurement are included in this standard.

1.6 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety, health, and environmental practices and determine the applicability of regulatory limitations prior to use.

1.7 This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for the Development of International StandardDetails, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee.

General Information

Status : ACTIVE
Standard Type: Main
Document No: ASTM E2009 : 23
Document Year: 2023
Pages: 6
  • Section Volume:
  • 14.01 Volume 14.01 Healthcare Informatics

Life Cycle

Currently Viewing

ACTIVE
ASTM E2009 : 23

Historical

Historical

Historical
Knowledge Corner

Expand Your Knowledge and Unlock Your Learning Potential - Your One-Stop Source for Information!

© Copyright 2026 BSB Edge Private Limited.

Enquire now +