1.1 This test method describes the determination of thermal conductivity, thermal diffusivity, and thermal effusivity of homogeneous, non-porous solid materials in the range of 0.10 W/(K·m) to 1.0 W/(K·m) by modulated temperature differential scanning calorimeter. This range includes many polymeric, glass, and ceramic materials. Thermal diffusivity, which is related to thermal conductivity through specific heat capacity and density, may also be derived. Thermal effusivity, conductivity, and diffusivity can be determined at one or more temperatures over the range of 0 °C to 90 °C.

1.2 The values stated in SI units are the standard.

1.3 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety, health, and environmental practices and determine the applicability of regulatory limitations prior to use.

1.4 This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for the Development of International Standards, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee.

General Information

Status : Historical
Standard Type: Main
Document No: ASTM E1952 : 25
Document Year: 2025
Pages: 8
  • Section Volume:
  • 14.01 Volume 14.01 Healthcare Informatics
  • ICS:
  • 17.200 Thermodynamics and temperature measurements

Life Cycle

Currently Viewing

Historical
ASTM E1952 : 25

Historical

Historical

Historical

Historical

Historical
Knowledge Corner

Expand Your Knowledge and Unlock Your Learning Potential - Your One-Stop Source for Information!

© Copyright 2026 BSB Edge Private Limited.

Enquire now +