logo

Standards Manage Your Business

We Manage Your Standards

ASTM

ASTM D6186 : 08(2013) New ASTM DRM Policy

Standard Test Method for Oxidation Induction Time of Lubricating Oils by Pressure Differential Scanning Calorimetry (PDSC)

Standard Details

1.1 This test method covers the determination of oxidation induction time of lubricating oils subjected to oxygen at 3.5 MPa (500 psig) and temperatures between 130 and 210°C.

1.2 The values stated in SI units are to be regarded as standard. No other units of measurement are included in this standard.

1.2.1 Exception—Pressure measurement appears in MPa with psig provided in parentheses for information only.

1.3 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.

General Information

Status : Historical
Standard Type: Main
Document No: ASTM D6186 : 08(2013)
Document Year: 2008
Pages: 5
  • Section Volume:
  • 05.02 Volume 05.02 Petroleum Products, Liquid Fuels, and Lubricants (II): D3711-D6122
  • ICS:
  • 75.100 Lubricants, industrial oils and related products

Life Cycle

Currently Viewing

Historical
ASTM D6186 : 08(2013)

Historical
Knowledge Corner

Expand Your Knowledge and Unlock Your Learning Potential - Your One-Stop Source for Information!

© Copyright 2026 BSB Edge Private Limited.

Enquire now +