1.1 This test method covers the determination of purity by use of differential scanning calorimetry and the evaluation of the results using the van't Hoff equation.

1.2 This test method is generally applicable to thermally stable compounds with well-defined melting temperatures.

1.3 Determination of purity by this test method is only applicable when the impurity dissolves in the melt and is insoluble in the crystal.

1.4 Computer- or electronic-based instruments, techniques, or data treatments equivalent to this test method may also be used.

Note 1--Since all data treatments are not equivalent, it is the responsibility of the user to verify equivalency prior to use.

1.5 SI values are the standard.

1.6 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.

1.6 There is no ISO method equivalent to this method.

General Information

Status : Historical
Standard Type: Main
Document No: ASTM E928 : 96
Document Year: 1996
Pages: 4
  • Section Volume:
  • 14.01 Volume 14.01 Healthcare Informatics

Life Cycle

Historical

Historical

Historical

Currently Viewing

Historical
ASTM E928 : 96
Knowledge Corner

Expand Your Knowledge and Unlock Your Learning Potential - Your One-Stop Source for Information!

© Copyright 2026 BSB Edge Private Limited.

Enquire now +