Standard Practice for Temperature Calibration of Differential Scanning Calorimeters and Differential Thermal Analyzers

Standard Details

1. Scope

1.1 This test method describes the temperature calibration of differential thermal analyzers and differential scanning calorimeters over the temperature range from 40 to +2500 C.

1.2

1.3 This test method is similar to ISO standard 11357-1.

This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use. Specific precautionary statements are given in Section .

General Information

Status : Historical
Standard Type: Main
Document No: ASTM E967 : 08
Document Year: 2008
Pages: 4
  • Section Volume:
  • 14.01 Volume 14.01 Healthcare Informatics

Life Cycle

Currently Viewing

Historical
ASTM E967 : 08

Historical

Historical
Knowledge Corner

Expand Your Knowledge and Unlock Your Learning Potential - Your One-Stop Source for Information!

© Copyright 2026 BSB Edge Private Limited.

Enquire now +