Standard Practice for Preparation and Use of Direct Tension Stress-Corrosion Test Specimens

Standard Details

1.1 This practice covers procedures for designing, preparing, and using ASTM standard tension test specimens for investigating susceptibility to stress-corrosion cracking. Axially loaded specimens may be stressed quantitatively with equipment for application of either a constant load, constant strain, or with a continuously increasing strain.

1.2 Tension test specimens are adaptable for testing a wide variety of product forms as well as parts joined by welding, riveting, or various other methods.

1.3 The exposure of specimens in a corrosive environment is treated only briefly because other StandardDetails are being prepared to deal with this aspect. Meanwhile, the investigator is referred to Practices G 35, G 36, G 37, and G 44, and to ASTM Special Technical Publication 425 ().

General Information

Status : Historical
Standard Type: Main
Document No: ASTM G49 : 85(2005)
Document Year: 1985
Pages: 6
  • Section Volume:
  • 03.02 Volume 03.02 Corrosion of Metals; Wear and Erosion

Life Cycle

Currently Viewing

Historical
ASTM G49 : 85(2005)
Knowledge Corner

Expand Your Knowledge and Unlock Your Learning Potential - Your One-Stop Source for Information!

© Copyright 2026 BSB Edge Private Limited.

Enquire now +