Standard Practice for Heat Flow Calibration of Differential Scanning Calorimeters

Standard Details

1.1 This practice covers the heat flow calibration of differential scanning calorimeters over the temperature range from -130°C to +800°C.

1.2 This practice may involve the use of hazardous materials, operations, and equipment. It is the responsibility of whoever uses this standard to establish appropriate safety practices, and to determine the applicability of regulatory limitations prior to use.

1.3 Values given in SI units are to be regarded as the standard. Where appropriate, traditional values and units may appear in parenthesis following the SI designations.

1.4 Computer or electronic based instruments, techniques or data manipulation equivalent to this practice may also be used.

1.5 This standard does not purport to address all of the safety problems associated with its use. It is the responsibility of whoever uses this standard to consult and establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use. See also Section 6.

General Information

Status : Historical
Standard Type: Main
Document No: ASTM E968 : 99
Document Year: 1999
Pages: 5
  • Section Volume:
  • 14.01 Volume 14.01 Healthcare Informatics

Life Cycle

Historical

Currently Viewing

Historical
ASTM E968 : 99
Knowledge Corner

Expand Your Knowledge and Unlock Your Learning Potential - Your One-Stop Source for Information!

© Copyright 2026 BSB Edge Private Limited.

Enquire now +