logo

Standards Manage Your Business

We Manage Your Standards

ASTM

ASTM D6604 : 00(2017) New ASTM DRM Policy

Standard Practice for Glass Transition Temperatures of Hydrocarbon Resins by Differential Scanning Calorimetry

Standard Details

1.1 This practice covers determination of glass transition temperatures of hydrocarbon (HC) resins by differential scanning calorimetry (DSC).

1.2 This practice is applicable to HC resins as defined in Terminology D6640. The normal operating temperature range is from the cryogenic region to approximately 180°C. The temperature range can be extended.

1.3 The values stated in SI units are to be regarded as standard. No other units of measurement are included in this standard.

1.4 Further discussion of glass transition can be found in Test Method D3418, and Test Method E1356.

1.5 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety, health, and environmental practices and determine the applicability of regulatory limitations prior to use.

1.6 This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for the Development of International StandardDetails, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee.

General Information

Status : Historical
Standard Type: Main
Document No: ASTM D6604 : 00(2017)
Document Year: 2000
Pages: 4
  • Section Volume:
  • 06.03 Volume 06.03 Paint -- Pigments, Polymers, Resins, Naval Stores, Cellulosic Esters, and Ink Vehicles

Life Cycle

Currently Viewing

Historical
ASTM D6604 : 00(2017)

Historical
Knowledge Corner

Expand Your Knowledge and Unlock Your Learning Potential - Your One-Stop Source for Information!

© Copyright 2026 BSB Edge Private Limited.

Enquire now +