1.1 This practice covers the determination of the amount of creep of metal-to-metal adhesive bonds due to the combined effects of temperature, tensile shear stress, and time.

Note 1-Since the characteristics that render a material resistant to creep under the condition of test are not yet completely known, the details of the procedure considered herein are those known to have important influences. Since other equally important characteristics may be discovered in the future, the recommended details are largely advisory in nature.

1.2 Test periods depend upon the reasonable life expected from the material in service. The uncertainties of extrapolation should be considered in deciding upon the length of the test.

1.3 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of whoever uses this standard to consult and establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.

General Information

Status : Historical
Standard Type: Main
Document No: ASTM D1780 : 99
Document Year: 1999
Pages: 4
  • Section Volume:
  • 15.06 Volume 15.06 Adhesives

Life Cycle

Historical

Currently Viewing

Historical
ASTM D1780 : 99
Knowledge Corner

Expand Your Knowledge and Unlock Your Learning Potential - Your One-Stop Source for Information!

© Copyright 2026 BSB Edge Private Limited.

Enquire now +