logo

Standards Manage Your Business

We Manage Your Standards

ASTM

ASTM E1829 : 02 New ASTM DRM Policy

Standard Guide for Handling Specimens Prior to Surface Analysis

Standard Details

1.1 This guide covers specimen handling and preparation prior to surface analysis and applies to the following surface analysis disciplines:

1.1.1 Auger electron spectroscopy (AES),

1.1.2 X-ray photoelectron spectroscopy (XPS or ESCA), and

1.1.3 Secondary ion mass spectrometry, SIMS.

1.1.4 Although primarily written for AES, XPS, and SIMS, these methods may also apply to many surface-sensitive analysis methods, such as ion scattering spectrometry, low-energy electron diffraction, and electron energy loss spectroscopy, where specimen handling can influence surface-sensitive measurements.

1.2 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.

General Information

Status : Historical
Standard Type: Main
Document No: ASTM E1829 : 02
Document Year: 2002
Pages: 5
  • Section Volume:
  • 03.06 Volume 03.06 Molecular Spectroscopy and Separation Science; Surface Analysis
  • ICS:
  • 71.040.50 Physicochemical methods of analysis

Life Cycle

Historical

Currently Viewing

Historical
ASTM E1829 : 02
Knowledge Corner

Expand Your Knowledge and Unlock Your Learning Potential - Your One-Stop Source for Information!

© Copyright 2026 BSB Edge Private Limited.

Enquire now +