ISO 15614-13:2005

Specification and qualification of welding procedures for metallic materials — Welding procedure test — Part 13: Resistance butt and flash welding

Standard Details

ISO 15614-13:2005 specifies the tests which should be used for qualification of welding procedure specifications.

It applies to resistance butt welding and flash welding of metallic materials, e.g. with solid, tubular, flat or circular cross-section. The basic principles of ISO 15614-13:2005 may be applied to other resistance welding processes when this is specified in the specification.

ISO 15614-13:2005 defines the conditions for carrying out tests and the limits of validity of a qualified welding procedure for all practical welding operations covered by ISO 15614-13:2005.

ISO 15614-13:2005 covers the following resistance welding processes as defined in ISO 4063:

24 flash welding using direct current or alternating current with various movement sequences, constant flashing and pulsed flashing;

25 resistance butt welding, using direct current or alternating current with various pressure sequences.

General Information

Status : WITHDRAWN
Standard Type: Main
Document No: ISO 15614-13:2005
Document Year: 2005
Pages: 15
Edition: 1
  • Section Volume:
  • ISO/TC 44/SC 6. Resistance welding and allied mechanical joining

Life Cycle

Currently Viewing

WITHDRAWN
ISO 15614-13:2005
Knowledge Corner

Expand Your Knowledge and Unlock Your Learning Potential - Your One-Stop Source for Information!

© Copyright 2026 BSB Edge Private Limited.

Enquire now +