logo

Standards Manage Your Business

We Manage Your Standards

ISO

ISO 15614-1:2004

Specification and qualification of welding procedures for metallic materials — Welding procedure test — Part 1: Arc and gas welding of steels and arc welding of nickel and nickel alloys

Standard Details

ISO 15614-1:2004 specifies how a preliminary welding procedure specification is qualified by welding procedure tests.

It defines the conditions for the execution of welding procedure tests and the range of qualification for welding procedures for all practical welding operations within a range of variables. Additional tests may be required by application StandardDetails.

ISO 15614-1:2004 applies to the arc and gas welding of steels in all product forms and the arc welding of nickel and nickel alloys in all product forms.

Arc and gas welding are covered by the following processes:

manual metal arc welding (metal-arc welding with covered electrode);

self-shielded tubular-cored arc welding;

submerged arc welding;

metal inert gas welding, MIG welding;

metal active gas welding, MAG welding;

tubular-cored metal arc welding with active gas shield;

tubular-cored metal arc welding with inert gas shield;

tungsten inert gas arc welding; TIG welding;

plasma arc welding;

oxy-acetylene welding.

The principles of ISO 15614-1:2004 may be applied to other fusion welding processes.

General Information

Status : WITHDRAWN
Standard Type: Main
Document No: ISO 15614-1:2004
Document Year: 2004
Pages: 28
Edition: 1
  • Section Volume:
  • ISO/TC 44/SC 10. Unification of requirements in the field of metal welding

Life Cycle

Currently Viewing

WITHDRAWN
ISO 15614-1:2004
Knowledge Corner

Expand Your Knowledge and Unlock Your Learning Potential - Your One-Stop Source for Information!

© Copyright 2026 BSB Edge Private Limited.

Enquire now +