logo

Standards Manage Your Business

We Manage Your Standards

ISO

ISO 15610:2023

Specification and qualification of welding procedures for metallic materials — Qualification based on tested welding consumables

Standard Details

This document specifies how a welding procedure can be qualified by using tested welding consumable data. It expands on the requirements given in ISO 15607.

In addition, it gives the range of qualification.

Application of this document is limited to parent material groups 1.1, 8.1, 21, 22.1 and 22.2 in accordance with ISO/TR 15608, which produce acceptable microstructures and properties in the heat-affected zone which do not deteriorate significantly in service.

This document is limited to:

    parent material thicknesses t ≤ 40 mm (groups 1.1 and 8.1) and t ≤ 20 mm (groups 21, 22.1 and 22.2);

    fillet welds with throat thickness a ≥ 1 mm.

This document is not applicable when any of the following is specified for the welded joint:

a)      hardness;

b)      impact properties;

c)       preheating;

d)      controlled heat input;

e)      interpass temperature;

f)       post-weld heat treatment.

The use of this document can also be restricted by an application standard, specification or other documents.

General Information

Status : WITHDRAWN
Standard Type: Main
Document No: ISO 15610:2023
Document Year: 2023
Pages: 6
Edition: 2
  • Section Volume:
  • ISO/TC 44/SC 10. Unification of requirements in the field of metal welding

Life Cycle

Currently Viewing

WITHDRAWN
ISO 15610:2023
Knowledge Corner

Expand Your Knowledge and Unlock Your Learning Potential - Your One-Stop Source for Information!

© Copyright 2026 BSB Edge Private Limited.

Enquire now +