ISO 16432:2006

Resistance welding — Procedure for projection welding of uncoated and coated low carbon steels using embossed projection(s)

Standard Details

ISO 16432:2006 specifies requirements for embossed-resistance-projection welding in the fabrication of assemblies of uncoated and metallic coated low carbon steel comprising two thicknesses of metal, where the maximum single sheet thickness of components to be welded is within the range 0,4 mm to 3 mm for the following materials:

  • uncoated steels;
  • hot-dip zinc or iron-zinc alloy (galvannealed) coated steel;
  • electrolytic zinc, zinc-iron, or zinc-nickel coated steel;
  • aluminium coated steel;
  • zinc-aluminium coated steel.

Organic coated or primer coated steels are not covered by ISO 16432:2006.

General Information

Status : Published
Standard Type: Main
Document No: ISO 16432:2006
Document Year: 2006
Pages: 15
Edition: 1
  • Section Volume:
  • ISO/TC 44/SC 6. Resistance welding and allied mechanical joining

Life Cycle

Currently Viewing

Published
ISO 16432:2006
Knowledge Corner

Expand Your Knowledge and Unlock Your Learning Potential - Your One-Stop Source for Information!

© Copyright 2026 BSB Edge Private Limited.

Enquire now +