ISO 11357-6:2008

Plastics — Differential scanning calorimetry (DSC) — Part 6: Determination of oxidation induction time (isothermal OIT) and oxidation induction temperature (dynamic OIT)

Standard Details

ISO 11357-6:2008 specifies methods for the determination of oxidation induction time (isothermal OIT) and oxidation induction temperature (dynamic OIT) of polymeric materials by means of differential scanning calorimetry (DSC). It is applicable to polyolefin resins that are in a fully stabilized or compounded form, either as raw materials or finished products. It may be applicable to other plastics.

General Information

Status : WITHDRAWN
Standard Type: Main
Document No: ISO 11357-6:2008
Document Year: 2008
Pages: 12
Edition: 2

Life Cycle

Currently Viewing

WITHDRAWN
ISO 11357-6:2008
Knowledge Corner

Expand Your Knowledge and Unlock Your Learning Potential - Your One-Stop Source for Information!

© Copyright 2026 BSB Edge Private Limited.

Enquire now +