logo

Standards Manage Your Business

We Manage Your Standards

ISO

ISO 7539-6:2003

Corrosion of metals and alloys — Stress corrosion testing — Part 6: Preparation and use of pre-cracked specimens for tests under constant load or constant displacement

Standard Details

ISO 7539-6:2002 covers procedures for designing, preparing and using pre-cracked specimens for investigating susceptibility to stress corrosion. It gives recommendations for the design, preparation and use of pre-cracked specimens for investigating susceptibility to stress corrosion.

The term "metal" as used in this part of ISO 7539 includes alloys.

Because of the need to confine plasticity at the crack tip, pre-cracked specimens are not suitable for the evaluation of thin products such as sheet or wire and are generally used for thicker products including plate bar and forgings. They can also be used for parts joined by welding.

General Information

Status : WITHDRAWN
Standard Type: Main
Document No: ISO 7539-6:2003
Document Year: 2003
Pages: 38
Edition: 2
  • Section Volume:
  • ISO/TC 156. Corrosion of metals and alloys
  • ICS:
  • 77.060 Corrosion of metals

Life Cycle

WITHDRAWN

Currently Viewing

WITHDRAWN
ISO 7539-6:2003
Knowledge Corner

Expand Your Knowledge and Unlock Your Learning Potential - Your One-Stop Source for Information!

© Copyright 2026 BSB Edge Private Limited.

Enquire now +