Corrosion of metals and alloys — Evaluation of pitting corrosion

Standard Details

Gives guidance on the selection of procedures that can be used in the identification and examination of pits and in the evaluation of pitting corrosion.

General Information

Status : WITHDRAWN
Standard Type: Main
Document No: ISO 11463:1995
Document Year: 1995
Pages: 10
Edition: 1
  • Section Volume:
  • ISO/TC 156. Corrosion of metals and alloys
  • ICS:
  • 77.060 Corrosion of metals