ISO 8181:2023

Atomic layer deposition — Vocabulary

Standard Details

This document defines general terms and film growth processes for atomic layer deposition (ALD). ALD technique is classified into conventional time separated ALD and spatial ALD according to the separation between sequential surface reactions of precursors on substrate. Besides planar substrate, ALD can be used for coating on micro-nano particles, which is developed as powder ALD. Some energy enhanced ALD techniques are also included. This document specifies the processes of different ALD methods.

This document applies to the process of ALD. This document does not apply to the deposited materials or specific nanostructures.

This document applies to industrial production, scientific research, teaching, publishing and scientific and technological communications related to ALD.

General Information

Status : Published
Standard Type: Main
Document No: ISO 8181:2023
Document Year: 2023
Pages: 10
Edition: 1
  • Section Volume:
  • ISO/TC 107. Metallic and other inorganic coatings

Life Cycle

Currently Viewing

Published
ISO 8181:2023
Knowledge Corner

Expand Your Knowledge and Unlock Your Learning Potential - Your One-Stop Source for Information!

© Copyright 2026 BSB Edge Private Limited.

Enquire now +