Thermal insulation — Test methods for specific heat capacity of thermal insulation for buildings in the high temperature range — Differential scanning calorimetry (DSC) method

Standard Details

This document specifies test methods for specific heat capacity under high temperature conditions from the normal temperature range to 1 600 K for insulation materials for buildings using the differential scanning calorimetry (DSC) method.

General Information

Status : Published
Standard Type: Main
Document No: ISO 24144:2023
Document Year: 2023
Pages: 21
Edition: 1
  • ICS:
  • 91.120.10 Thermal insulation of buildings