logo

Standards Manage Your Business

We Manage Your Standards

ASTM

ASTM E2253 : 21 New ASTM DRM Policy

Standard Test Method for Temperature and Enthalpy Measurement Validation of Differential Scanning Calorimeters

Standard Details

1.1 This test method provides procedures for validating temperature and enthalpy measurements of differential scanning calorimeters (DSC) and analytical methods based upon the measurement of temperature or enthalpy (or heat), or both, by DSC. Performance parameters determined include temperature and calorimetric repeatability (precision), detection limit, quantitation limit, linearity, and bias. This test method is applicable to exothermic events.

1.2 Validation of apparatus performance and analytical methods is requested or required for quality initiatives or where results may be used for legal purposes.

1.3 The values stated in SI units are to regarded as standard. No other units of measurement are included in this standard.

1.4 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety, health, and environmental practices and determine the applicability of regulatory limitations prior to use.

1.5 This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for the Development of International StandardDetails, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee.

General Information

Status : ACTIVE
Standard Type: Main
Document No: ASTM E2253 : 21
Document Year: 2021
Pages: 7
  • Section Volume:
  • 14.01 Volume 14.01 Healthcare Informatics

Life Cycle

Currently Viewing

ACTIVE
ASTM E2253 : 21

Historical

Historical

Historical
Knowledge Corner

Expand Your Knowledge and Unlock Your Learning Potential - Your One-Stop Source for Information!

© Copyright 2026 BSB Edge Private Limited.

Enquire now +