Standard Practice for Making and Using Precracked Double Beam Stress Corrosion Specimens

Standard Details

1.1 This practice covers procedures for fabricating, preparing, and using precracked double beam stress corrosion test specimens. This specimen configuration was

General Information

Status : ACTIVE
Standard Type: Main
Document No: ASTM G168 : 17
Document Year: 2017
Pages: 10
  • Section Volume:
  • 03.02 Volume 03.02 Corrosion of Metals; Wear and Erosion
  • ICS:
  • 77.060 Corrosion of metals