Specification for approval testing of welders when welding procedure approval is not required - Fusion welding of steel

Standard Details

Covers the approval testing of welders for manual or semi-automatic fusion welding of ferritic or austenitic stainless steels when welding procedure approval is not required. There is a choice of 9 test welds covering sheet, plate and pipe, with requirements for examination and testing.

General Information

Status : Confirmed
Standard Type: Main
Document No: BS 4872-1:1982
Document Year: 1982
Pages: 28
  • Section Volume:
  • GBM15 Metal Treatment & Welding (GMB15)
  • ICS:
  • 25.160.01 Welding, brazing and soldering in general