Status : Withdrawn
Standard Type : Main
Document Year : 2007
Pages : 21
Edition : 1
ISO 15614-7:2007 specifies how a preliminary welding procedure specification for overlay welding is qualified by welding procedure tests.
ISO 15614-7:2007 defines the conditions for carrying out welding procedure tests and the range of qualification for welding procedures for all practical welding operations within the range of variables listed in Clause 8.
Additional tests may be required by application StandardDetails.
ISO 15614-7:2007 applies to all welding processes suitable for overlay welding.
ISO 15614-7:2007 is applicable to all new welding procedures. However, it does not invalidate previous welding procedure tests made to former national StandardDetails or specifications. Where additional tests are carried out to make the qualification technically equivalent, they are only done on a test piece made in accordance with ISO 15614-7:2007.
ISO 15614-7:2007 does not apply to overlay welding where cracks are intentionally produced (e.g. special hardfacing applications).