Specification and qualification of welding procedures for metallic materials — Welding procedure test — Part 12: Spot, seam and projection welding

Standard Details

This document specifies the tests which can be used for qualification of welding procedure specifications for spot, seam, and projection welding processes.

NOTE       The procedures are written for embossed projection welding. They can be adapted for solid projections as well, e.g. nut welding, stud welding. cross wire welding.

This document defines the conditions for carrying out tests and the limits of validity of a qualified welding procedure for all practical welding operations covered by this document.

It covers the following resistance welding processes, as defined in ISO 4063:

—    21 – resistance spot welding;

—    211 – indirect spot welding;

—    212 – direct spot welding;

—    22 – resistance seam welding;

—    221 – lap seam welding;

—    222 – mash seam welding;

—    223 – Prep-lap seam welding;

—    224 – Wire seam welding;

—    225 – foil butt-seam welding;

—    226 – seam welding with strip;

—    23 – projection welding;

—    231 – indirect projection welding;

—    232 – direct projection welding.

General Information

Status : Published
Standard Type: Main
Document No: ISO 15614-12:2021
Document Year: 2021
Pages: 7
Edition: 3
  • Section Volume:
  • ISO/TC 44/SC 6. Resistance welding and allied mechanical joining

Life Cycle

Currently Viewing

Published
ISO 15614-12:2021
Knowledge Corner

Expand Your Knowledge and Unlock Your Learning Potential - Your One-Stop Source for Information!

© Copyright 2026 BSB Edge Private Limited.

Enquire now +