IEC 61395:1998 (EN-FR)

Overhead electrical conductors - Creep test procedures for stranded conductors

Standard Details

Is applicable to non-interrupted creep-testing of stranded conductors for overhead lines such as those specified by IEC 61089. Procedures for interpreting the results are also included. The object of the test is principally to calculate creep for any purpose and to compare creep of different conductors.

General Information

Status : ACTIVE
Standard Type: Main
Document No: IEC 61395:1998 (EN-FR)
Document Year: 1998
Pages: 21
Edition: 1.0
  • Section Volume:
  • TC 7 Overhead electrical conductors
  • ICS:
  • 29.240.20 Power transmission and distribution lines