SAE ARP1110D : 2021

Minimizing Stress Corrosion Cracking in Wrought Forms of Steels and Corrosion Resistant Steels and Alloys

Standard Details

The purpose of this SAE Aerospace Recommended Practice (ARP) is to provide the aerospace industry with recommendations concerning the minimization of stress corrosion cracking in wrought heat-treatable carbon and low alloy steels and in austenitic, precipitation hardenable, and martensitic corrosion-resistant steels and alloys.The detailed recommendations are based on laboratory and field experience and reflect those design practices and fabrication procedures which should avoid in-service stress corrosion cracking.

Cross Reference: AFML-TR-68-115,AMS2430,AMS2431,AMS2432,ASTMG49,ASTMG58,MCIC-HB-01

General Information

Status : Revised
Standard Type: Main
Document No: SAE ARP1110D : 2021
Document Year: 2021
Pages: 5

Life Cycle

Currently Viewing

Revised
SAE ARP1110D : 2021
Knowledge Corner

Expand Your Knowledge and Unlock Your Learning Potential - Your One-Stop Source for Information!

© Copyright 2025 BSB Edge Private Limited.

Enquire now +