Mineral insulating oils - Characterization of paraffinic/naphthenic nature - Low temperature differential scanning calorimetry (DSC) test method

Standard Details

Describes a test method for the classification of mineral insulating oils as either paraffinic or naphthenic, by means of low-temperature differential scanning calorimetry (DSC). For the purpose of this technical report, the typical operating temperature range extends from -100 °C to +100 °C. The temperature range can be extended, depending upon the instrumentation used. The method is applicable to mineral insulating oils obtained from petroleum crudes. It may be also applied to mineral oils containing pour point depressants, as these additives do not prevent the formation of paraffin crystals but only the growing of such micro-crystals.

General Information

Status : ACTIVE
Standard Type: Main
Document No: IEC TR 61946:2007 (EN-FR)
Document Year: 2007
Pages: 27
Edition: 1.0
  • Section Volume:
  • TC 10 Fluids for electrotechnical applications

Life Cycle

Currently Viewing

ACTIVE
IEC TR 61946:2007 (EN-FR)
Knowledge Corner

Expand Your Knowledge and Unlock Your Learning Potential - Your One-Stop Source for Information!

© Copyright 2026 BSB Edge Private Limited.

Enquire now +