BS 5131-1.1:1991

Methods of test for footwear and footwear materials. Adhesives - Resistance of adhesive joints to heat (creep test)

Standard Details

Method for measuring resistance when subjected to a constant peeling force at a controlled elevated temperature over a timed interval.