Metallic materials — Verification of static uniaxial testing machines — Part 2: Tension creep testing machines — Verification of the applied force

Standard Details

ISO 7500-2:2006 specifies the verification of testing machines used for uniaxial creep testing in tension in accordance with ISO 204.

The verification consists of

  • a general inspection of the testing machine, and
  • a verification of the force applied by the testing machine.

ISO 7500-2:2006 applies to dead-weight machines, lever-type creep testing machines and direct-spring-loading machines.

Machines with a force-measuring system should be verified in accordance with ISO 7500-1.

General Information

Status : Published
Standard Type: Main
Document No: ISO 7500-2:2006
Document Year: 2006
Pages: 17
Edition: 2

Life Cycle

Currently Viewing

Published
ISO 7500-2:2006
Knowledge Corner

Expand Your Knowledge and Unlock Your Learning Potential - Your One-Stop Source for Information!

© Copyright 2026 BSB Edge Private Limited.

Enquire now +