Corrosion of metals and alloys — Stress corrosion testing — Part 5: Preparation and use of C-ring specimens

Standard Details

Covers procedures for designing, preparing, stressing, exposing and inspecting C-ring specimens. These versatile, economical specimens may be used to test a variety of product forms including parts joined by welding. C-ring specimens may be stressed to predeterminded levels, using simple equipment for application of either constant load or constant strain.

General Information

Status : Published
Standard Type: Main
Document No: ISO 7539-5:1989
Document Year: 1989
Pages: 9
Edition: 1
  • Section Volume:
  • ISO/TC 156. Corrosion of metals and alloys
  • ICS:
  • 77.060 Corrosion of metals

Life Cycle

Currently Viewing

Published
ISO 7539-5:1989
Knowledge Corner

Expand Your Knowledge and Unlock Your Learning Potential - Your One-Stop Source for Information!

© Copyright 2026 BSB Edge Private Limited.

Enquire now +