Corrosion of metals and alloys — Guidelines for assessing the significance of stress corrosion cracks detected in service

Standard Details

ISO 21601:2013 provides guidelines on the appropriate steps to take when a stress corrosion crack has been detected in service and an assessment has to be made of the implications for structural integrity.

Such an evaluation should be made in the context of the perceived consequences of failure using appropriate risk-based management methodologies. Since this is application-specific, it is beyond the scope of ISO 21601:2013.

General Information

Status : Published
Standard Type: Main
Document No: ISO 21601:2013
Document Year: 2013
Pages: 19
Edition: 1
  • Section Volume:
  • ISO/TC 156. Corrosion of metals and alloys
  • ICS:
  • 77.060 Corrosion of metals

Life Cycle

Currently Viewing

Published
ISO 21601:2013
Knowledge Corner

Expand Your Knowledge and Unlock Your Learning Potential - Your One-Stop Source for Information!

© Copyright 2026 BSB Edge Private Limited.

Enquire now +